EFFECT OF WELD REPAIR EXCAVATION SIZE OF DEFECTIVE PORTION OF MAIN GAS PIPELINES ON TIME OF PREHEATING DURING WELD BUILD-UP REPAIR

UDC: 622.691.4.004.67
DOI: -

Authors:

Volkov Igor V.,
Elagina Oksana Ju.


Keywords: preheating, weld build-up repair, duration of interoperation period, metal cooling rate

Annotation:

The effect of the size of weld repair excavation of the defective portion of main gas pipelines on the metal cooling rate after preheating in the process of weld build-up repair is studied. The parameters of the heated portion cooling during preheating for patch repair are measured. The calculated and experimental values are compared. The need to regulate the maximum duration of the interoperation period according to excavation parameters, ambient temperature and method of heating is shown.

Bibliography:

1. Фролов В.В. Теория сварочных процессов: Учебник для вузов/В.Н. Волченко, В.М. Ямпольский, В.А. Винокуров и др.; Под ред. В.В. Фролова. — М.: Высш. шк., 1988. — 559 с.
2. Теория сварочных процессов: Учебник для вузов/А.В. Коновалов, А.С. Куркин, Э.Л. Макаров, В.М. Неровный, Б.Ф. Якушин; Под ред. В.М. Неровного. — М.: Изд-во МГТУ имени Н.Э. Баумана, 2007. — 752 с.
3. СТО Газпром 2-2.2-137-2007 (Часть II). Инструкция по технологиям сварки при строительстве и ремонте промысловых и магистральных газопроводов. — М., 2007. — 177 с.
4. Царьков А.В., Лоскутов С.В., Труханов К.Ю., Подхалюзин П.С. Разработка системы газопламенного подогрева участка трубы магистрального газопровода в условиях автоматизированного процесса ремонта поверхностных дефектов//Сварка и диагностика. — 2014. — № 6. — С. 31–34.